◆Nickel200 waa ganacsi saafi ah (99.6%) oo ka samaysan nikkel, kaas oo leh sifooyin farsamo oo aad u wanaagsan iyo iska caabin daxalka aad u fiican, kulaylka iyo korantada sare, content gaas hooseeya iyo cadaadiska uumiga hooseeya.

◆Nickel201 (N02201) waa nikkel ganacsi saafi ah oo ka kooban kaarboon aad u yar, waxaa la ansixiyay in ay u adeegto deegaanka ilaa 1230 ℃.

Halabuurka kiimikada

Darajo

Ni

Fe

Cu

C

Mn

S

Si

Nickel200

99

≤0.4

≤0.25

≤0.15

≤0.35

≤0.01

≤0.35

Nickel201

99

≤0.4

≤0.25

≤0.02

≤0.35

≤0.01

≤0.35

Hantida Alloy ugu yar

qaabka alaabta

xaalad

xoogga xajinta RmN/m㎡

Xoogga Wax-soo-saarka Rp0.2N/m㎡

Kordhinta sida%

adkaanta Brinell HB

ul iyo xariijimo

kulul duuban

60-85

15 ilaa 45

35-55

45-80

ul iyo xariijimo

qabow la sawiray ama la tirtiray

55-75

15 ilaa 30

40-55

45-70

saxan

nuugista

55-80

15 ilaa 40

40 ~ 60

45-75

caleenta

nuugista

55-75

15 ilaa 30

40-55

70ka ugu sarreeya

Dhuumaha birta

nusqaan lahayn

55-75

12 ilaa 30

40 ~ 60

70ka ugu sarreeya