Hastelloy
Daawaha Heerkulka Sare
◆Hastelloy B waa alloy u adkaysta yaraynta daxalka dhexdhexaadka ah, oo ku habboon sulfuric acid kulul iyo aaladaha gaaska chloride hydrogen iyo qaybaha.
◆Hastelloy B-2 waxa ay leedahay qaab-dhismeedka crystal cubic oo weji ku dhisan.Xakamaynta waxa ku jira birta iyo chromium ilaa ugu yaraan, waxay yaraynaysaa habacsanaanta habaynta waxayna ka hortagtaa roobabka wajiga Ni4Mo inta u dhaxaysa 700-870°C.Waxaa inta badan loo adeegsadaa kimistari, kiimikaad batroolka, soosaarka tamarta iyo goobta xakamaynta wasakhowga.
◆Hastelloy B-3 waxa uu leeyahay iska caabin aad u wanaagsan oo daxalka u leh heerkul kasta iyo fiirsashada hydrochloric acid.
◆Hastelloy C waxa uu leeyahay adayg wanaagsan iyo iska caabin daxalka at 650-1040 ℃.
◆Hastelloy C-4 waa daawaha u adkaysta redox qaab-dhismeedka daxalka ka kooban ion koloride, oo uu leeyahay xasilloonida kulaylka wanaagsan.Waxaa loo isticmaalaa aaladaha koloriin ee koloriin qoyan, aashitada hypochlorous, sulfuric acid, hydrochloric acid, iyo asiidh isku dhafan.Waxaa si toos ah loo codsadaa alxanka ka dib.
◆Hastelloy C-22 waa daawaha ka kooban molybdenum, tungsten iyo chromium, kaas oo si weyn loogu isticmaalo beeraha kiimikaad iyo petrochemical, iyo injineernimada hababka kiimikada kala duwan oo leh oksidation iyo sifooyinka dhimista.
◆Hastelloy C-276 waxay leedahay iska caabin godad heer sare ah, iska caabin daxalka uniform, iska caabin daxalka intergranular iyo sifooyinka farsamo heer-sare wanaagsan.Waxaa inta badan loo adeegsadaa warshadaha nukliyeerka, kiimikooyinka, batroolka, iyo warshadaha birta ee aan birta ahayn.
◆Hastelloy C -2000 waa daxalka u adkaysta ugu dhamaystiran, kaas oo uu leeyahay iska caabin aad u fiican in daxalka labis ee labada oxidizing iyo dhimista deegaanka.
◆HastelloyG-3 waxay leedahay iska caabin daxalka oo ka wanaagsan iyo xasilloonida kulaylka, waxayna leedahay waxqabad wanaagsan oo ku jira phosphoric acid iyo warbaahinta kale ee isku dhafan ee oksaydhaynta.
◆HastelloyX waxay leedahay iska caabin daxalka sare leh waxayna ku habboon tahay warshadaha mashiinada kala duwan ee jawi acidic ah.
Halabuurka kiimikada
Darajo | C | P | S | Mn | Si | Ni | Cr | Co | Cu | Fe | N | Mo | Al | W | V | Ti | kale |
aan ka weynayn | |||||||||||||||||
HastelloyB | 0.05 | 0.04 | 0.03 | 1 | 1 | saldhig | ≤1 | ≤2.5 | - | 4~6 | - | 26 ilaa 30 | - | - | 0.2 ilaa 0.4 | - | - |
HastelloyB-2 | 0.02 | 0.04 | 0.03 | 1 | 0.1 | saldhig | ≤1 | ≤1 | - | ≤2 | - | 26 ilaa 30 | - | - | - | - | |
HastelloyB -3 | 0.01 | 0.04 | 0.03 | 3 | 0.1 | ≥65 | 1~3 | ≤3 | ≤0.2 | 1~3 | - | 27-32 | ≤0.5 | ≤3 | ≤0.2 | ≤0.2 | - |
HastelloyC | 0.08 | 0.04 | 0.03 | 1 | 1 | saldhig | 14.5 ilaa 16.5 | ≤2.5 | - | 4~7 | - | 15 ilaa 17 | - | 3 4.5 | ≤0.35 | - | - |
HastelloyC-4 | 0.015 | 0.04 | 0.03 | 1 | 0.08 | saldhig | 14 ilaa 18 | ≤2 | - | ≤3 | - | 14 ilaa 17 | - | - | - | ≤0.7 | - |
HastelloyC-22 | 0.015 | 0.025 | 0.01 | 0.5 | 0.08 | saldhig | 20-22.5 | ≤2.5 | - | 2~6 | - | 12.5 ilaa 14.5 | - | 2.5 ilaa 3.5 | ≤0.35 | - | - |
HastelloyC-276 | 0.01 | 0.04 | 0.03 | 1 | 0.08 | saldhig | 14.5 ilaa 16.5 | ≤2.5 | - | 4~7 | - | 15 ilaa 17 | - | 3 4.5 | ≤0.35 | - | - |
HastelloyC -2000 | 0.01 | 0.025 | 0.01 | 0.5 | 0.08 | saldhig | 22 ilaa 24 | ≤2 | 1.3-1.9 | 3 | - | 15 ilaa 17 | ≤0.5 | - | - | - | - |
HastelloyG -3 | 0.015 | 0.03 | 0.03 | 1 | 1 | saldhig | 21-23.5 | ≤5 | 1.5 ilaa 2.5 | 18 ilaa 21 | - | 6 ~8 | - | ≤1.5 | - | - | Nb/Ta0.3~1.5 |
HastelloyX | 0.1 | 0.025 | 0.015 | 1 | 1 | saldhig | 20.5 ilaa 23 | 0.5 ilaa 2.5 | - | 17-20 | - | 8 ilaa 10 | ≤0.5 | 0.2~1 | - | ≤0.15 | - |
Hantida Alloy ugu yar
Darajo | gobol | xoogga xajinta RmN/m㎡ | Xoogga Wax-soo-saarka Rp0.2N/m㎡ | Kordhinta sida% | adkaanta Brinell HB |
HastelloyB | xal adag | 690 | 310 | 40 | - |
HastelloyB-2 | xal adag | 690 | 310 | 40 | - |
HastelloyB -3 | xal adag | 690 | 290 | 42 | - |
HastelloyC | xal adag | 690 | 300 | 41 | - |
HastelloyC-4 | xal adag | 650 | 280 | 40 | - |
HastelloyC-22 | xal adag | 690 | 283 | 40 | - |
HastelloyC-276 | xal adag | 690 | 283 | 40 | - |
HastelloyC -2000 | xal adag | 700 | 290 | 40 | - |
HastelloyG -3 | xal adag | 700 | 300 | 40 | - |
HastelloyX | xal adag | 725 | 310 | 30 | - |