Birta aan Lahayn 904L 1.4539

Faahfaahinta Alaabta

Tags Product

Codsiga

Warshada kiimikaad, warshada saliida, dhirta batroolka, taangiyada bleaching ee warshadaha waraaqaha, dhirta sunta gubta, codsiga biyaha badda, sulfuric iyo phosphoric acid. Sababtoo ah nuxurka C-yar ee hooseeya, iska caabinta daxalka intergranular ayaa sidoo kale lagu dammaanad qaaday xaaladda alxanka.

Waxyaabaha Kiimikada ah

Curiyaha % La joogo (qaab wax soo saarka)
Kaarboon (C) 0.02
Silikoon (Si) 0.70
Manganese (Mn) 2.00
Fosfooraska (P) 0.03
Sulfur (S) 0.01
Chromium (Cr) 19.00 - 21.00
Nickel (Ni) 24.00 - 26.00
Nitrojiin (N) 0.15
Molybdenum (Mo) 4.00 - 5.00
Copper (Cu) 1.20 - 2.00
Birta (Fe) Dheelitiran

Guryaha makaanikada

Qalabka makaanikada (heerkulka qolka ee xaalad la baab'iyay)

  Foomka Alaabta
  C H P L L TW/TS
Dhumucda (mm) Max. 8.0 13.5 75 160 2502) 60
Xoogga Wax-soo-saarka Rp0.2 N/mm2 2403) 2203) 2203) 2304) 2305) 2306)
Rp1.0 N/mm2 2703) 2603) 2603) 2603) 2603) 2503)
Xoogga Jilicsan N/mm2 530 - 7303) 530 - 7303) 520 - 7203) 530 - 7304) 530 - 7305) 520 - 7206)
Dheeraynta min. gudaha % Jmin (Longitudinal) - 100 100 100 - 120
Jmin (Tranverse) - 60 60 - 60 90

Xogta tixraaca

Cufnaanta 20°C kg/m3 8.0
Heerarka kulaylka W/m K at 20°C 12
Qaabka Elasticity kN/mm2 at 20°C 195
200°C 182
400°C 166
500°C 158
Awoodda kulaylka gaarka ah 20°CJ/kg K 450
Iska caabin koronto ah 20°C Ω mm2/m 1.0

 

Habaynta / alxanka

Habka alxanka caadiga ah ee darajadan birta ah waa:

  • TIG-alxanka
  • MAG-Alxanka Silig Adag
  • Alxanka Arc (E)
  • Alxanka Bean Laser
  • Alxanka Arc-ga quusta (SAW)

Markaad dooranayso birta buuxinta, culayska daxalka waa in sidoo kale la tixgeliyaa. Isticmaalka biraha buuxinta alxanka sare waxay noqon kartaa lagama maarmaan sababtoo ah qaabka kabka ee birta alxanka. Kuleyliyaha hore uma baahna birtaan. Daawaynta kulaylka ka dib alxanka caadiyan caadiyan maaha. Biraha Austenitic-ku waxay leeyihiin kaliya 30% kulaylka kuleyliyaha birta aan daawaha lahayn. Barta isku dhafka ahi way ka hoosaysaa birta aan daawaynta lahayn sidaa darteed biraha austenitic waa in lagu lingaxo kulaylka hoose marka loo eego birta aan daawaynta lahayn. Si aad uga fogaato kulaylka ama gubashada go'yaal khafiif ah, xawaaraha alxanka sare waa in la mariyaa. Taarikada naxaasta ah ee loogu talagalay diidmada kuleyliyaha degdega ah ayaa shaqeynaya, halka, si looga fogaado dildilaaca birta alxanka, looma oggola in ay dusha sare ku fidiso saxanka naxaasta ah. Birtani waxay leedahay iskudhaf aad u sarreeya oo balaadhinta kulaylka ah sida birta aan daawaynta lahayn. Marka la eego kororka kulaylka xun, qallooc weyn waa in la filayaa. Marka alxanka 1.4539 dhammaan hababka, kuwaas oo ka soo horjeeda qalloocan this (tusaale dib-tallaabada isku xigxiga alxanka, alxanka beddelka ah ee dhinacyada iska soo horjeeda leh laba-V dabada alxanka, meelaynta laba alxanka marka qaybaha ay sidaas u weyn) waa in si gaar ah loo ixtiraamo. Dhumucdiisuna waxay ka badan tahay 12mm alxanka dabada laba-V waa in la door bidaa halkii laga heli lahaa alxanka dabada-hal-V. Xagasha lagu daray waa in ay ahaataa 60°-70°, marka la isticmaalayo MIG-alxanka qiyaastii 50° ayaa ku filan. Waa in laga fogaadaa ururinta tolida alxanka. Alxanka tuubada waa in lagu dhejiyaa masaafo aad uga gaaban midba midka kale (oo aad uga gaaban kuwan birta aan daawaha lahayn), si looga hortago qallafsanaan xoog leh, soo gaabinaya ama jajabinaya alxanka taarka. Xirmooyinka waa in la shiido ama ugu yaraan ay ka xoroobaan dildilaaca. 1.4539 ee la xidhiidha birta alxanka austenitic iyo galinta kulaylka aadka u sarreeya ee qabatinka si loo sameeyo dildilaaca kulaylka ayaa jira. Qabatinka dildilaaca kulaylka waa la xaddidi karaa, haddii birta alxanka ay ka kooban tahay waxyaabo hoose oo ferrite ah (delta ferrite). Waxyaabaha ku jira ferrite ilaa 10% waxay leeyihiin saameyn wanaagsan mana saameeyaan caabbinta daxalka guud ahaan. Lakabka ugu khafiifsan ee suurtogalka ah waa in la lingaxo (farsamo kuul adag) sababtoo ah xawaaraha qaboojinta sare wuxuu yareeyaa qabatinka dildilaaca kulul. Qaboojin degdeg ah oo wanaagsan waa in la hiigsadaa marka la alxanayo sidoo kale, si looga fogaado u nuglaanshaha daxalka intergranular iyo embrittlement. 1.4539 aad bay ugu habboon tahay alxanka alxanka laysarka (weldability A si waafaqsan wargayska DVS 3203, qaybta 3). Iyada oo ballac alxanka ah oo ka yar 0.3mm siday u kala horreeyaan 0.1mm dhumucdiisuna waxay tahay isticmaalka biraha buuxinta daruuri ma aha. Iyada oo leh godad alxanka weyn, birta buuxinta la mid ah ayaa la isticmaali karaa. Iyada oo laga fogaanayo oksaydhka gudaha tolitaanka alxanka leysarka alxanka dhabarka ee lagu dabaqi karo, tusaale ahaan helium sida gaas aan shaqaynayn, tollaynta alxanku waxay u adkaysataa sida birta salka. Khatar dildilaac ah oo kulul ee tollaynta alxanka ma jirto, marka aad dooranayso hab lagu dabaqi karo. 1.4539 waa alos ku habboon goynta fiyuuska laysarka leh ee nitrogen ama ololka oo ogsijiin. Cidhifyada la gooyay kaliya waxay leeyihiin aagag kuleyl yar saameeya oo guud ahaan waa ka xor dildilaaca mirco-da sidaas darteed si fiican ayey u qaabaysan yihiin. Marka la dooranayo hababka lagu dabaqi karo, geesaha la gooyey fiyuuska ayaa si toos ah loo beddeli karaa. Gaar ahaan, waa la alxan karaa iyada oo aan wax diyaargaraw kale ah la helin. Marka la farsameeyo oo keliya qalabka aan-xawaalka ahayn sida burushka birta, pneumatic-ka iyo wixii la mid ah waa la oggol yahay, si aanay khatar u gelin qulqulka. Waa in la dayacay in lagu calaamadiyo gudaha tolitaanka alxanka oo leh boolal oleaginous ah ama heerkul muujinaya midabyo. Iska caabbinta daxalka sare ee birtaan aan daxalka lahayn waxay ku salaysan tahay samaynta lakab aan toos ahayn oo dusha sare ah. Midabbada, miisaanka, haraaga dharbaaxada, birta taraamka, spatters iyo wixii la mid ah waa in la saaraa, si aan loo baabi'in lakabka dadban. Nadiifinta dusha sare waxaa lagu dabaqi karaa habsocodyada cadayashada, shiididda, qajaarka ama qarxinta (ciidda silica-free-birta ama muraayadaha) Si loo cadaydo kaliya burushyada birta ah ee aan birta lahayn ayaa loo isticmaali karaa. Soo saarista aagga tolitaanka ee hore loo cadayday waxaa lagu fuliyaa iyada oo la durayo oo la buufiyo, si kastaba ha ahaatee, inta badan koollada la jarjaray ama xalalka ayaa la isticmaalaa. Ka dib marka la qaado biyo si taxadar leh loogu dhaqay waa in la sameeyaa.