Nimonic

Faahfaahinta Alaabta

Tags Product

Daawaha Heerkulka Sare

◆ Nimonic90 waxa ay leedahay xoog xajin sare leh iyo iska caabin gurguurta, iska caabin oksaydh oo wanaagsan iyo iska caabin daxalka, waxayna ku habboon tahay saxanadaha marawaxadaha, daabyada iyo xajiyayaasha heerkulka sare ee matoorada marawaxadaha.
◆ Nimonic91 wuxuu leeyahay awood sare iyo waxqabadka anti-oxidation heerkulka sare ee 650-1000 ° C, wuxuuna ku habboon yahay qaybaha heerkulku sarreeyo sida mishiinka hawada, matoorada gantaallada, iyo quwadda nukliyeerka.

Halabuurka kiimikada

Darajo

C

Si

Mn

S

P

Cr

Ni

Fe

Cu

Ti

Al

Co

kale

aan ka weynayn

Nimonic90

0.13

1

1

0.015

 

18 ilaa 21

saldhig

≤1.5

≤0.2

2~3

1~2

15 ilaa 21

hogaanka≤0.002 B≤0.02 Zr≤0.15

Nimonic91

0.1

1

1

0.015

 

27-30

saldhig

≤1

≤0.5

1.9 ilaa 2.7

0.9 ilaa 1.5

19-21

Nb0.4~1.1 B0.002~0.01 Zr≤0.1

Hantida Alloy ugu yar

Darajo

gobol

xoogga xajinta RmN/m㎡

Xoogga Wax-soo-saarka Rp0.2N/m㎡

Kordhinta sida%

adkaanta Brinell HB

Nimonic90

Daaweynta xalalka

780

550

7

-

Nimonic91

Daaweynta xalalka

820

590

8

-