  • ALLOY 600 XOGTA ALAAB AH

    INCONEL 600

    Inconel Alloy 600 A nickel-chromium alloy oo leh caabbinta oksaydhaynta wanaagsan ee heerkulka sare iyo iska caabinta chloride-ion stress-corrosion dildilaaca, daxalka biyo saafi ah oo sarreeya, iyo daxalka caustic. Loo isticmaalo qaybaha foornada, kiimikooyinka iyo habaynta cuntada, injineernimada nukliyeerka, iyo ololka dabka.

    UNS: N06600

    W.Nr.: 2.4816

  • ALLOY 825 XOGTA ALAABKA

    Shirkadda Sandmeyer Steel waxay kaydisaa Alloy 825 saxan alloy nickel ah oo dhumucdiisuna tahay .1875″ (4.8mm) ilaa 2.00″ (50.8mm) ee codsiyada u adkaysta daxalka ee xakamaynta wasakhowga hawada, kiimikaad iyo kiimikaad batroolka, diyaarinta cuntada, nukliyeerka, saliidda xeebaha iyo soosaarka gaaska , farsamaynta macdanta, sifaynta batroolka, warshadaynta birta iyo qashinka.

  • Qaabaysan, Flat, Square, Wareeg ah, Fiican, Dahaaran oo Bare Wire ASTM A167, AMS 5523

    Alloy 310S waa austenitic chromium nickel ahama oo leh iska caabin oksaydh oo wanaagsan iyo xoog heerkulka sare ee adeega joogtada ah ilaa 2000ºF (oo la bixiyo yaraynta gaasta baaruudda aan la joogin). Waxa kale oo loo istcimaalaa adeega kala go'a heerkulka ilaa 1900F sababtoo ah waxay ka hortagtaa dib-u-cusboonaynta waxayna leedahay koronto yar oo balaadhin ah. Arintani waxay yaraynaysaa u janjeera birta inay ku rogmato adeega kulaylka. Alloy 310S waxay la mid tahay daawaha 310 marka laga reebo kaarboonka hoose ee ka kooban si loo yareeyo roobabka carbide inta lagu jiro alxanka.

  • ALLOY 625 XOGTA ALAABKA

    Alloy 625 waa aan magnetic , daxalka - iyo oxidation u adkaysta, daawaha ku salaysan nikkel. Awoodeeda aadka u wanaagsan iyo adayga heerkulka kala duwan ee cryogenic ilaa 2000°F (1093°C) waxa ay asal ahaan ka soo jeedaan saamaynta xalka adag ee biraha refractory, kolumbium iyo molybdenum, oo ku jira matrix nikkel-chromium. Daawadu waxay leedahay daal aad u wanaagsan iyo iska caabin dildilaac ah oo ka dhan ah ion chloride. Qaar ka mid ah codsiyada caadiga ah ee daawaha 625 ayaa waxaa ku jiray gaashaaman kulaylka, qalabka foornada, marinnada mishiinka marawaxadaha gaaska, mashiinnada dabka iyo baararka buufinta, qalabka dhirta kiimikada, iyo codsiyada biyaha badda ee gaarka ah.

  • ALLOY 718 XOGTA ALAABKA

    Inconel Alloy 718 Roobab-adkegi kara nikkel-chromium alloy sidoo kale ka kooban xaddi aad u badan oo bir, niobium, iyo molybdenum oo ay la socdaan xaddi yar oo aluminium iyo titanium. Waxay isku daraysaa iska caabin daxalka iyo xoog sare leh alxanka heer sare ah oo ay ku jirto iska caabin dildilaaca dambe. Daawadu waxay leedahay awood aad u fiican oo gurguurta oo heerkulkeedu yahay 1300°F (700°C). Loo isticmaalo marawaxadaha gaaska, matoorada gantaallada, dayax-gacmeedyada, reactors nukliyeerka, bambooyin, iyo qalabaynta. INCONEL alloy 718SPF™ waa nooc gaar ah oo ah INCONEL alloy 718, oo loogu talagalay samaynta superplastic.

    UNS: N07718

    W.Nr.: 2.4668

  • Alloy

    Heerkulka Sare ee Aloy Kiimikada Halabuurka Darajada C Si Mn SP Cr Ni Fe Al Ti Cu Mo Nb aan ka weynayn Inconel600 0.15 0.5 1 0.015 0.03 14~17 saldhiga 25 saldhiga 0.2 0.35 0...